Aerosol Can Corrosion: Causes, Types, and Prevention

Aerosol can corrosion is an important packaging compatibility issue for product developers and aerosol brands. Corrosion can affect the container’s appearance, product quality, storage stability, and, in more serious cases, package integrity.

The risk depends on several interacting factors: the metal container, its internal protective coating, the aerosol formulation, and the storage environment. A formulation that works well in one container may not perform the same way in another.

Understanding these interactions helps brands select suitable packaging and identify potential compatibility problems before mass production.

What Causes Aerosol Can Corrosion?

Corrosion develops when a metal surface reacts with substances in its surrounding environment. In aerosol packaging, this environment may include the product formulation inside the can or moisture and other contaminants on its external surface.

Several factors can contribute to aerosol can corrosion:

  • Formulation ingredients: Certain solvents, acids, alkaline ingredients, salts, and other reactive substances may interact with metal surfaces or protective coatings.
  • Water content: Water can contribute to corrosion in some metal-container and formulation systems, particularly when other corrosive substances are present.
  • pH: Strongly acidic or alkaline formulations may create compatibility challenges, depending on the metal and coating system.
  • Chloride and other ions: Certain ions can increase corrosion risk under specific conditions.
  • Internal coating defects: Discontinuities, damage, or inadequate coating coverage may expose the underlying metal.
  • Storage conditions: Moisture, condensation, temperature changes, and prolonged exposure can influence corrosion development.

However, no single ingredient determines the outcome. A water-based or acidic formulation does not automatically corrode every aerosol can. The complete formulation, metal substrate, coating system, and storage conditions must be evaluated together.

Research published in the Journal of Intelligent Manufacturing identifies formulation ingredients, water contamination, pH, container materials, and coatings as relevant factors in aerosol packaging compatibility. Read the packaging compatibility study.

Types of Corrosion in Aerosol Cans

Corrosion can develop on different parts of an aerosol container. Its appearance and location help explain the possible cause, although visual inspection alone cannot establish the full extent of a compatibility problem.

Internal Corrosion

Internal corrosion develops on the inside surface of the aerosol container, where the formulation contacts the metal or its protective coating.

If the formulation interacts with an exposed metal area, corrosion may develop beneath or around the coating. Depending on the material and reaction, this can lead to discoloration, localized metal damage, or changes in package integrity.

Internal corrosion deserves particular attention because the affected surface remains in contact with the product throughout storage. Corrosion products may also contaminate the formulation or affect its appearance and performance.

External Corrosion

External corrosion affects the outside surface of the can. Unlike internal corrosion, it does not necessarily result from direct contact with the product formulation.

Potential contributing factors include:

  • High humidity or prolonged exposure to moisture
  • Condensation during storage or transportation
  • Damaged exterior coatings or protective finishes
  • Product leakage or residue around the container
  • Unsuitable storage conditions, particularly in persistently damp environments

External corrosion may initially appear as rust spots, surface discoloration, or deterioration of the exterior finish. Its significance depends on the location and extent of the damage.

It is also important to distinguish container corrosion from corrosion that an aerosol spray may cause on an external surface after application. These are different issues and require different evaluations.

Pitting Corrosion and Coating Defects

Not all corrosion spreads evenly across a metal surface.

General corrosion affects a relatively broad area, while localized corrosion develops at specific points. Pitting corrosion is a localized form that creates small cavities in the metal surface.

Internal polymer coatings may also show defects such as blistering, discontinuities, or loss of adhesion. These conditions can expose the underlying metal and create potential sites for corrosion.

A packaging compatibility study discusses general corrosion, detinning, pitting, and internal coating blistering as distinct aerosol packaging defects. Importantly, not every visible coating imperfection indicates that a finished package will fail during normal storage. Springer packaging compatibility research.

How Aerosol Can Materials and Internal Coatings Affect Corrosion

Metal selection is an important part of aerosol packaging development. The two common metal materials are tinplate steel and aluminum. Both offer useful packaging properties, but their corrosion behavior differs.

Tinplate Steel

Tinplate aerosol cans use a steel substrate with a thin tin layer. Manufacturers may also apply an internal protective lacquer to separate the formulation from the metal surface.

The tin layer and internal coating serve different functions. The coating helps protect the container from the formulation, while the tin layer forms part of the metal substrate’s protective system.

If the internal coating contains defects or does not suit the formulation, the exposed areas may become vulnerable to corrosion. The behavior also depends on the formulation and the condition of the tinplate.

Aluminum

Aluminum aerosol cans are commonly produced as seamless, one-piece containers. Aluminum naturally forms a thin oxide layer on its surface, which provides some corrosion resistance.

However, aluminum is not immune to chemical attack. Certain formulations, particularly those with unsuitable chemical conditions, may still interact with the metal. Internal coatings can therefore remain important depending on the product and packaging specification.

Why Internal Coatings Matter

Internal lacquers create a protective barrier between the formulation and the metal container. Their effectiveness depends on the coating chemistry, coverage, adhesion, and compatibility with the product.

A coating suitable for one formulation may not perform equally well with another. The manufacturing process and container design also matter because forming operations and seams can influence coating integrity.

For a broader comparison of container structures and material options, see our guide to aerosol can materials.

How to Prevent Aerosol Can Corrosion

Preventing corrosion starts during product development. Brands should evaluate the complete aerosol package rather than selecting a container based on material or appearance alone.

Consider these practical steps:

  1. Select a suitable container material. Compare tinplate and aluminum according to the formulation, product requirements, and intended storage conditions.
  2. Evaluate formulation compatibility. Review potentially reactive ingredients, water content, pH, and other relevant formulation characteristics.
  3. Check internal coating suitability. Confirm that the selected coating system is appropriate for the formulation and container construction.
  4. Review all packaging components. The valve, mounting cup, seals, and other wetted components may also interact with the formulation.
  5. Conduct appropriate compatibility evaluations. Assess the filled product and packaging system before approving commercial production.
  6. Monitor storage and product condition. Check for visible corrosion, coating changes, leakage, discoloration, and dispensing abnormalities during development and evaluation.

These steps reduce avoidable compatibility risks, but no single material choice or protective coating guarantees that corrosion cannot occur.

Brands should also consider the complete aerosol packaging options available for their product rather than treating the container as an isolated component.

Why Compatibility Testing Matters for Aerosol Products

Compatibility and stability evaluations help determine whether a formulation and its packaging system can work together under the intended conditions.

Depending on the product, relevant observations may include:

  • Visible corrosion, rust, or pitting
  • Changes in internal coating condition
  • Formulation discoloration or other physical changes
  • Package leakage or loss of integrity
  • Weight or pressure loss
  • Changes in dispensing performance

Different tests answer different technical questions.

Internal coating coverage assessment examines whether the protective coating covers the intended metal surface. FEA 651 provides methods for assessing internal coating coverage in metal aerosol containers and valve mounting cups. The standard specifically states that these methods are not intended to predict the potential shelf life of new formulations. FEA 651 – Assessment of Internal Coating Coverage.

Compatibility evaluations examine how the formulation interacts with the container, coating, valve, and other packaging components. They help identify potential corrosion and other package-related defects.

Long-term preservation evaluations examine product and package behavior over time. FEA 603 provides guidelines for testing long-term preservation and measuring weight loss. It should not be confused with a dedicated internal coating coverage or corrosion test. The European Aerosol Federation maintains a list of relevant industry standards, including FEA 603 and FEA 651. FEA Standards.

Accelerated evaluations can help identify potential problems during development, but their results should not be converted into a guaranteed real-time shelf life using a universal time ratio. Appropriate evaluation plans depend on the formulation, packaging system, and intended product requirements.

Choosing the Right Aerosol Manufacturing Partner

Formulation and packaging decisions should develop together. A change in ingredients may affect container compatibility, while a different can material or coating may require further evaluation.

An experienced manufacturing partner can help coordinate these decisions before mass production. This includes reviewing formulation requirements, matching packaging components, preparing samples, and checking the production process.

TENTOP CHEM, the brand of Zhongshan Tentop Fine Chemical Co., Ltd., supports aerosol OEM/ODM projects through formulation development and adjustment, aerosol filling, BOV production, liquid filling, and packaging coordination.

The company operates four high-speed aerosol filling lines, three BOV production lines, and two liquid filling lines. Its project workflow includes pre-production sample evaluation, production-process checks, and final inspection before shipment.

For brands seeking support with product development and manufacturing, TENTOP CHEM provides aerosol contract manufacturing services. Specialized corrosion testing and can-coating manufacture are not presented as in-house services; these requirements should be discussed with the relevant packaging or testing suppliers.

Conclusion

Aerosol can corrosion results from interactions between metal surfaces, protective coatings, product formulations, and environmental conditions. Internal corrosion, external corrosion, pitting, and coating defects can affect packaging in different ways.

The most reliable approach is to evaluate the complete aerosol system during product development. Suitable material selection, coating compatibility, formulation review, and appropriate stability and compatibility evaluations can help identify risks before mass production.

If you are developing a new aerosol product, discuss your formulation and packaging requirements with TENTOP CHEM to plan the manufacturing process and coordinate suitable packaging options.

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top